硬質薄膜 | 足立研究室 論文データベース

Hard Coating
Number Title Authors Paper Page Keyword1
32 "The Fundamental Wear Properties of Plasma-Sprayed Alumina Coating Film in Lubricated Condition", Z. Z. Li, K. Kato and K. Hokkirigawa, Journal of JSME ©, 52 (1986), 3285-3291. Wear, Coating, Hard coating
71 "The Critical Loads for the Generation of Hertzian and Lateral Cracks in the Ceramic Coating Films", D. F. Diao, K. Hokkirigawa and K. Kato, Proceedings of the Japan International Tribology Conference Nagoya, 1990, 1 (1990), 1-6. Fracture, Coating, Hard coating
84 "Transitions of Microscopic Wear Mechanism for Cr2O3 Ceramic Coatings During Repeated Sliding Observed in a Scanning Electron Microscope Tribosystem", H. Kitsunai, K. Hokkirigawa, N. Tsumaki and K. Kato, Wear, 151 (1991), 279-290. Ceramics, Coating, Wear, SEM-Tribosystem, Hard coating
85 "The Wear Mechanism of Ceramic Coating Film in Repeated Sliding Friction", K. Kato, D. F. Diao and M. Tsutsumi, Wear of Material, ASME (1991), 243-248. Ceramics, Coating, Wear, SEM-Tribosystem, Hard coating
95 "Transitions of Microscopic Wear Mechanism for Cr2O3 Ceramic Coatings during Repeated Sliding Observed in a Scanning Electron-microscope Tribosystem", H. Kitsunai, K. Hokkirigawa, N. Tsumaki and K. Kato, Wear, 15 (1991), 279-289. Ceramics, Coating, Wear, SEM-Tribosystem, Hard coating
102 "The Local Yield Map of Hard Coating under Sliding Contact", D. F. Diao, K. Kato and K. Hayashi, Proceedings of the 19th Leeds-Lyon Symposium on Tribology (1992), 419-427. Coating, Wear, MAP, Hard coating
114 "Sliding Contact Mechanism of Hard Coating", K. Kato and D. F. Diao, ASME Winter Annual Meeting, PED67/Trib. 4 (1993), 243-248. Hard coating, Wear
115 "The Maximum Tensile Stress on a Hard Coating under Sliding Friction", D. F. Diao, K. Kato and K. Hayashi, Tribology International, 27, 4 (1994), 267-272. Hard coating
123 "Interface Yield Map of a Hard Coating under Sliding Contact", D. F. Diao and K. Kato, Thin Solid Films, 245 (1994), 115-121. Hard coating, MAP
124 "Spalling Mechanism of Al2O3 Ceramic Coating Coated WC-Co Substrate under Sliding Contact", D. F. Diao and K. Kato, Thin Solid Films, 245 (1994), 104-108. Hard coating, Wear
125 "Fracture Mechanisms of Ceramic Coatings in Indentation", D. F. Diao, K. Kato and K. Hokkirigawa, Transactions of the ASME, Journal of Tribology, 116 (1994), 860-869. Hard coating, Fracture
137 "Microwear Mechanisms of Coatings", K. Kato, Surface and Coating Technology, 76-77 (1995), 469-474. Wear, Coating, Review, Hard coating
138 "Fracture Mechanisms of Ceramic Coatings in Indentation", D. F. Diao, K. Kato and K. Hokkirigawa, Transactions of the ASME, Journal of Tribology, 116 (1994), 860-869. Coating, Fracture, Hard coating
157 "Review of Failure and Wear Mechanisms of Thin Hard CVD and PVD Coatings under Conditions of Abrasion, Erosion and Sliding", M. Olsson and K. Kato, Proceedings of the International Tribology Conference, Yokohama 1995 (1995), 575-580. Wear, Coating, Review, Hard coating
162 "Microtribological Characterization of Carbon Nitride Coatings", A. Khurshudov, K. Kato and D. Sawada, Proceedings of the International Tribology Conference, Yokohama 1995 (1995), 1931-1936. CN coating, hard coating
169 "Tribological and Mechanical Properties of Carbon Nitride Thin Coating Prepared by Ion-beam assisted Deposition", A. Khurshudov, K. Kato and D. Sawada, Tribology Letters, 2 (1996), 13-21. CN coating, hard coating
171 "Comparison of tribological properties of carbon and carbon nitride protective coatings over magnetic media", A. Khurshudov, K. Kato and D. Sawada, Journal of Vacuum Science and Technology, 14 (1996), 2935-2939. CN coating, Hard coating
175 "Microscopic Wear Mechanism of CVD TiN Coating", N. Umehara, B. H. Moon and K. Kato, Journal of JSME ©, 63, 608 (1997), 1336-1341. SEM-Tribosystem, Wear, Coating, Hard coating
177 "The Relationship between Microscopic Wear Properties and Wear Modes of CVD TiN Coating (Evaluation of Wear Properties with SEM VTR Tribosystem)", N. Umehara, B. H. Moon and K. Kato, Journal of JSME ©, 63, 610 (1997), 2082-2086. Wear, SEM-Tribosystem, Coating, Hard coating
182 "Micro-wear Mechanisms of Thin Hard Coatings Sliding Against Diamond Tip of AFM", K. Kato, H. Koide and N. Umehara, Proceedings International Conference on Mechatronics for Information and Precision Equipment, Tokyo (1997), 732-735. Wear, Coating, Atomic Force Microscopy (AFM), Hard coating
197 "Tribological Properties of Nano-meter Scale Hard Coatings", N. Umehara and K. Kato, Proceedings of International Symposium for High Performance of Tribosystem (1998), 41-46. Coating, Hard Coating
199 "Micro-wear Mechanisms of Thin Hard Coatings Sliding Against Diamond Tip of AFM", K. Kato, H. Koide and N. Umehara, Advances in Information Storage Systems (1998), 289-302. Wear, Coating, Atomic Force Microscopy (AFM), Hard coating
206 "The Effect of Internal Stress of CNx Coating on Its Wear in Sliding Friction", K. Kato, M. Bai, N. Umehara and Y. Miyake, Surface and Coating Technology, 113 (1999), 233-241. CN coating, Hard coating
213 "The Effect of Texture Height and a CNx Coating Thickness of Hard Disk Slider on Friction and Wear between Slider and Disk", L. Zhou, K. Kato, N. Umehara and Y. Miyake, Tribology International, 33 (2000), 665-672. CN coating, Hard coating, Texture, Hard disk (HD)
216 "Scratch-Wear Resistance of Nanoscale Super Thin Carbon Nitride Overcoat Evaluated by AFM with a Diamond Tip", M. Bai, K. Kato, N. Umehara, Y. Miyake, J. Xu and H. Tokisue, Surface and Coating Technology, 126 (2000), 181-194. CN coating, Hard coating, Wear, Atomic Force Microscopy (AFM)
217 "Micro-wear properties of carbon nitride coatings", K. Kato, H. Koide and N. Umehara, Wear, 238 (2000), 40-44. CN coating, Hard coating, Wear, Atomic Force Microscopy (AFM)
222 "Dependence of Microstructure and Nanomechanical Properties of Amorphous Carbon Nitride Thin Films on Vacuum Annealing", M. Bai, K. Kato, N. Umehara, Y. Miyake, J. Xu, H. Tokisue, Thin Solid Films, 376 (2000), 170-178. CN coating, Hard coating
223 "Nanoindentation and FEM Study of the Effect of Internal Stress on Micro/nano Mechanical Property of Thin CNx Films", M. Bai, K. Kato, N. Umehara, Y. Miyake, Thin Solid Films, 377-378 (2000), 138-147. CN coating, Hard coating
227 "Fatigue Properties of nm-Scale Thickness a-CNx and DLC Coatings Evaluated with AFM Scratch Fatigue Test", N. Umehara, M. Kawauchi, H. Koide and K. Kato, Proceedings of the International Tribology Conference Nagasaki, 2000, 1 (2001), 709-714. Wear, CN coating, Hard coating, Atomic Force Microscopy (AFM)
235 "Nitrogen Lubricated Sliding between CNx Coatings and Ceramic Balls", N. Umehara, M. Tatsuno and K. Kato, Proceedings of the International Tribology Conference Nagasaki, 2000, 2 (2001), 1007-1012. CN coating, Hard coating, N2 gas
257 "Nano-scale Fatigue Wear of Carbon Nitride Coating: Part II Wear Properties", D. F. Wang and K. Kato, Transactions of the ASME, Journal of Tribology, 125 (2003), 430-436. Wear, CN coating, Hard coating, SEM-Tribosystem
260 "Friction, wear and N2-lubrication of carbon nitride coatings: a review", K. Kato, N. Umehara and K. Adachi, Wear, 254 (2003), 1062-1069. CN coating, Hard coating, N2 gas
225 "Stiction of Textured and CNx Coated Slider in Glid Test", M. Bai, K. Kato, N. Umehara, L. Zhou and Y. Miyake Proceedings of 2000 Asia-Pacific Magnetic Recoarding Conference, Tokyo, Japan (2000), CN coating, Hard coating, Texture